Alloy 238.0 is a standard general purpose Al-Si-Cu alloy used for high hardness in the as-cast condition, good casting characteristics, and good machinability. This datasheet provides information on key alloy metallurgy, processing effects on typical properties, fabrication characteristics, and applications of this 2xxx series alloy.