Abstract

This datasheet provides information on key alloy metallurgy, processing effects on physical and mechanical properties, and application characteristics of Al-Si-Mg general-purpose die-casting alloys 360.0 and A360.0.

You do not currently have access to this chapter.
Don't already have an account? Register

360.0 and A360.0: Al-Si-Mg General-Purpose Die-Casting Alloys, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 558–559, https://doi.org/10.31399/asm.hb.v02b.a0006571