Skip to Main Content
Skip Nav Destination

Abstract

This article lists temper designations and their definitions for aluminum alloys along with their product forms used in the United States (ANSI H35.1), Europe (EN 515), and internationally (ISO 2107).

Abstract

This article provides a comprehensive matrix for selecting an aluminum filler alloy for the gas tungsten arc and gas metal arc welding processes, based on the various requirements or service conditions. A table lists the nominal strengths of aluminum filler metals.

Abstract

This article contains a table that lists the values of nominal compositions and composition limits of wrought aluminum alloys.

Abstract

This article contains a table that lists the values of nominal compositions and composition limits of aluminum alloy castings.