The development of aluminum alloys has progressed along two tracks: heat treatable and non-heat treatable. The Aluminum Association alloy composition limits and product temper are defined for major alloying elements. This article summarizes the historical evolution of the different series of wrought aluminum alloys (1xxx to 8xxx) and discusses their applications based on the alloying system introduced by the Aluminum Association.

Abstract

This article summarizes the characteristics, material properties, and typical applications of aluminum alloy wrought products. It describes the most widely used worldwide alloy designation system and discusses five major categories, namely flat-rolled products; rod, bar, and wire; tubular products; shapes; and forgings. The article also discusses three widely used indexes to define the fracture resistance of aluminum alloys: notch toughness, tear resistance, and plane-strain fracture toughness. It also describes three types of corrosion attack of these alloys: general or atmospheric surface corrosion, stress-corrosion cracking, and exfoliation attack.

You do not currently have access to this chapter.
Don't already have an account? Register
Close Modal

or Create an Account

Close Modal
Close Modal