This article is a compilation of tables that present information on austenitizing temperatures for direct-hardening carbon and alloy steels, case depth of steels for different carburizing times and temperatures, typical heat treatments for case hardening of carbon and carburizing of alloy steels, as well as direct hardening of carbon steels and alloy steels.