This article focuses on various heat treatment practices recommended for different types of high-speed tool steels. Commonly used methods include annealing, stress relieving, preheating, austenitizing, quenching, tempering, carburizing, and nitriding. The article describes hardening for various types of cutting tools, namely, broaches, chasers, milling cutters, drills, taps, reamers, form tools, and hobs, and for thread rolling dies, threading dies, and bearings.