Simulation of Steels Prone to Quench Cracking
-
Published:2014
Abstract
Quench cracking is a brittle fracture phenomenon, and its occurrence depends not only on the stress changes but also on the mechanical characteristics of metals. Simulation of quenching processes has become possible in the analysis of quench cracking. This article commences with a discussion on the studies conducted to determine the origin of quench cracks, and then describes various test procedures for determining the susceptibility of quench cracking. It provides a description of the brittle fracture in terms of fracture mechanics and fracture toughness of quenched metals, and discusses the effects of impurities, hydrogen, and surface roughness on cracking. The article exemplifies simulation works applied to several successful cracking tests on cylindrical and complex-shaped steel parts.
Sign in
ASM members
Member Sign InK. Arimoto, Simulation of Steels Prone to Quench Cracking, Heat Treating of Irons and Steels, Vol 4D, ASM Handbook, Edited By Jon L. Dossett, George E. Totten, ASM International, 2014, p 44–57, https://doi.org/10.31399/asm.hb.v04d.a0005938
Download citation file:
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.