The orientation of the devices within a package determine the best chosen approach for access to a select component embedded in epoxy both in package or System in Package and multi-chip module (MCM). This article assists the analyst in making decisions on frontside access using flat lapping, chemical decapsulation, laser ablation, plasma reactive ion etching (RIE), CNC based milling and polishing, or a combination of these coupled with optical or electrical endpoint means. This article discusses the general characteristics, advantages, and disadvantages of each of these techniques. It also presents a case study illustrating the application of CNC milling to isolate MCM leakage failure.

You do not currently have access to this chapter.
Don't already have an account? Register

Jim Colvin, 2019. "Frontside Sample Preparation", Microelectronics Failure Analysis: Desk Reference, Tejinder Gandhi

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal