Abstract

X-ray imaging systems have long played a critical role in failure analysis laboratories. This article begins by listing several favorable traits that make X-rays uniquely well suited for non-destructive evaluation and testing. It then provides information on X-ray equipment and X-ray microscopy and its application in failure analysis of integrated circuit (IC) packaging and IC boards. The final section is devoted to the discussion on nanoscale 3D X-ray microscopy and its applications.