This article introduces the wafer-level fault localization failure analysis (FA) process flow for an accelerated yield ramp-up of integrated circuits. It discusses the primary design considerations of a fault localization system with an emphasis on complex tester-based applications. The article presents examples that demonstrate the benefits of the enhanced wafer-level FA process. It also introduces the setup of the wafer-level fault localization system. The application of the wafer-level FA process on a 22 nm technology device failing memory test is studied and some common design limitations and their implications are discussed. The article presents a case study and finally introduces a different value-add application flow capitalizing on the wafer-level fault localization system.

You do not currently have access to this chapter.
Don't already have an account? Register

2019. "Failure Analysis Process and Management", Microelectronics Failure Analysis: Desk Reference, Tejinder Gandhi

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal