Heat-Transfer Equations[1]

Published:
2014
Page range:
481 - 514
Publication history
August 31, 2014

Abstract

This article is a comprehensive collection of formulas, tables, and analytical solutions, addressing hundreds of heat-transfer scenarios encountered in science and engineering. With detailed explanations and dimensioned drawings, the article demonstrates how to set up and solve real-world problems, accounting for material properties, environmental variables, boundary and state conditions, and the primary modes of heat transfer: conduction, convection, and radiation. The article also includes reference data and provides closed-form solutions for common heat-transfer applications such as insulated pipes, cooling fins, radiation shields, and composite structures and configurations.

You do not currently have access to this content.
Don't already have an account? Register

2014. "Heat-Transfer Equations", Steel Heat Treating Technologies, Jon L. Dossett, George E. Totten

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal