This article contains tables that provide values for compositions and physical and mechanical properties of 1xxx series aluminum alloys. Emphasis is placed on highly refined aluminum (1199) and high-purity aluminum (1060). Examples of common 1xxx series aluminum alloys specified in products standards are also presented. A figure illustrates the effect of purity on strength and hardness of unalloyed aluminum.

You do not currently have access to this chapter.
Don't already have an account? Register

2019. "1xxx Aluminum Alloy Datasheets", Properties and Selection of Aluminum Alloys, Kevin Anderson, John Weritz, J. Gilbert Kaufman