This datasheet provides information on key alloy metallurgy and processing effects on mechanical and corrosion performance properties of aluminum alloy 7449. A comparison of toughness and stress-corrosion cracking resistance of alloy 7449 with other alloys is also provided.

You do not currently have access to this chapter.
Don't already have an account? Register

2019. "7449: Very High-Strength Plate and Extrusion Alloy", Properties and Selection of Aluminum Alloys, Kevin Anderson, John Weritz, J. Gilbert Kaufman