This datasheet provides information on composition limits, fabrication characteristics, processing effects on physical and mechanical properties, and application performance of thick plate and forging alloy 7085. It presents the specified minimum strength and fracture properties for plate, die, and hand forgings. The datasheet provides a comparison of the strength, fracture toughness, and fatigue crack growth resistance of alloy 7085 plate with those of the legacy plate alloy 7050. It shows tensile yield and ultimate strength at elevated temperature for various temperatures and exposure times for 7085-T7452 die forgings.