Skip to Main Content

Abstract

The moderate-strength weldable alloy 5086 provides higher strength than alloy 5052 while maintaining good corrosion resistance in a marine environment. This datasheet provides information on key alloy metallurgy, processing effects on physical and tensile properties, product specifications, and fabrication characteristics of this 5xxx series alloy.

You do not currently have access to this chapter.
Don't already have an account? Register

2019. "5086 and Alclad 5086: Moderate-Strength Weldable Alloy", Properties and Selection of Aluminum Alloys, Kevin Anderson, John Weritz, J. Gilbert Kaufman