Alloy 6013 is a high-strength Al-Mg-Si-Cu alloy, developed for extruded automotive bumpers. This datasheet provides information on key alloy metallurgy, processing effects on physical, tensile, static and fracture properties, and fabrication characteristics of this 6xxx series alloy.