This datasheet provides information on key alloy metallurgy and applications of Alclad 2029. It contains tables that present statistically determined mechanical property minimums for Alclad 2029-T8 sheet and plate. The plane stress fracture toughness and fatigue crack growth resistance of alloys 2029 and 2024 are illustrated.