Alloy 7055 is widely used in the aerospace industry in applications as plate and extrusions. This datasheet provides information on key alloy metallurgy and processing effects on fracture, mechanical, tensile, and compressive properties of this 7xxx series alloy.

You do not currently have access to this chapter.
Don't already have an account? Register

2019. "7055: High-Strength Plate and Extrusion Alloy", Properties and Selection of Aluminum Alloys, Kevin Anderson, John Weritz, J. Gilbert Kaufman