The sheet alloys 6009 and 6010 fill the need for materials that would be formed in the soft T4 temper and age harden during the automotive paint-bake cycle. This datasheet provides information on key alloy metallurgy, processing effects on physical and mechanical properties, and fabrication characteristics of these 6xxx series alloys.