Alloy 365.0 and A365.0 are developed near eutectic Al-Si die-casting alloys with additions of manganese to reduce die soldering. This datasheet provides information on key alloy metallurgy, processing effects on tensile properties, and fabrication characteristics of these 3xxx series alloys.