Alloy 295.0 is an Al-Cu-Si alloy suitable for sand casting requiring high strength with ductility and toughness. This datasheet provides information on key alloy metallurgy, fabrication characteristics, processing effects on physical and mechanical properties, and applications of this series alloy. Room-temperature aging characteristics for aluminum alloy 295.0-F, -T4, -T6, and -T7 are also illustrated.