Abstract

This datasheet provides information on key alloy metallurgy, fabrication characteristics, mill-product specifications, processing effects on physical properties, and applications of high-strength alloy 2014. It contains tables that list values of tensile property limits for alloy 2014 flat product, rod, wire, bar, extrusions, and forgings.