Alloy 2198 is an Al-Cu-Li alloy that is used in combination with 2196-T8 stringers for the fuselage skins of the Bombardier C-Series. This datasheet provides information on composition limits of the alloy 2198 and provides a performance comparison of 2198-T8 and 2024-T351 alloys.