Abstract

Ferromagnetic resonance (FMR) is used in the identification of the magnetic state of materials, the quantitative determination of static magnetic parameters, and the determination of microwave losses. This article describes the theory of ferromagnetic resonance and provides information on reflection spectrometers, microwave spectrometers, and ferromagnetic anti-resonance spectrometers used for measuring FMR. It also discusses the applications of FMR and provides several detailed examples.