Failure of a Squeeze-Clamped Polyethylene Natural Gas Pipeline

By
Robert E. Jones, Jr
Robert E. Jones, Jr
The University of Texas at San Antonio
Search for other works by this author on:
;
Walter L. Bradley
Walter L. Bradley
Texas A&M University
Search for other works by this author on:
Published:
1993
Page range:
482 - 486

Abstract

A high-density polyethylene (HDPE) natural gas distribution pipe (Grade PE 3306) failed by slow, stable crack growth while in residential service. The leak occurred at a location where a squeeze clamp had been used to close the pipe during maintenance. Failure analysis showed that the origin of the failure was a small surface crack in the inner pipe wall produced by the clamping. Fracture mechanics calculations confirmed that the suspected failure process would result in a failure time close to the actual time to failure. It was recommended that: materials be screened for susceptibility to the formation of the inner wall cracks since it was not found to occur in pipe typical of that currently being placed in service; pipes be re-rounded after clamp removal to minimize residual stresses which caused failure; and a metal reinforcing collar be placed around the squeeze location after clamp removal.

You do not currently have access to this content.
Don't already have an account? Register

Robert E. Jones, Jr, Walter L. Bradley, 1993. "Failure of a Squeeze-Clamped Polyethylene Natural Gas Pipeline", Handbook of Case Histories in Failure Analysis, Khlefa A. Esaklul

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal