Skip to Main Content
ASM Failure Analysis Case Histories

Handbook of Case Histories in Failure Analysis

Edited by
Khlefa A. Esaklul
Khlefa A. Esaklul
Search for other works by this author on:
ASM International
Volume
2
ISBN electronic:
978-1-62708-215-0
Publication date:
1993
Book Chapter

Fatigue Failure of a Carbon Steel Piston Shaft on an Extrusion Press Billet-Loading Tray

By
Phillip Green
Phillip Green
University of Hull
Search for other works by this author on:
Published:
1993
Page range:
525 - 528

Abstract

A recurring piston shaft failure problem on the billet-loading tray of an extrusion press was investigated. Two shafts fractured within a period of 10 days. The shaft was machined from normalized EN3 (AISI C1022) steel stock without further treatment. Visual, microstructural, chemical, and mechanical (hardness and tensile properties) analyses of failed shaft specimens were conducted. The examinations showed that the shafts had failed by fatigue. It was recommended that a low-alloy steel (e.g., 3% Ni-Cr) in the hardened and tempered condition and subjected to shot-peening surface-hardening treatment be used. The provision of a stop to reduce bending stresses was also recommended.

You do not currently have access to this content.
Don't already have an account? Register

Phillip Green, 1993. "Fatigue Failure of a Carbon Steel Piston Shaft on an Extrusion Press Billet-Loading Tray", Handbook of Case Histories in Failure Analysis, Khlefa A. Esaklul

Download citation file: