Fatigue Failures of Connecting Bolts in a Truck Crane

By
Yoshio Kitsunai
Yoshio Kitsunai
National Research Institute of Industrial Safety
Search for other works by this author on:
;
Yutaka Maeda
Yutaka Maeda
National Research Institute of Industrial Safety
Search for other works by this author on:
Published:
1993
Page range:
419 - 424

Abstract

JIS SCM435 steel bolts that connected the slewing ring to the base carrier on a truck crane failed during the lifting of steel piles. The bolts were double-ended stud types and had been in operation for 5600 h. Failure occurred in the root of the external thread that was in contact with the first internal thread in the slewing ring. Examination of plastic carbon replicas indicated that failure was the result of fatigue action. Failure was attributed to overloading during service and increased stress concentration on a few bolts due to nonuniform separations around the slewing ring. A design change to achieve equal separation between bolt holes was recommended.

You do not currently have access to this content.
Don't already have an account? Register

Yoshio Kitsunai, Yutaka Maeda, 1993. "Fatigue Failures of Connecting Bolts in a Truck Crane", Handbook of Case Histories in Failure Analysis, Khlefa A. Esaklul

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal