Galvanic Corrosion Failure of Austenitic Stainless Steel Pipe Flange Assemblies

By
Edward C. Lochanski
Edward C. Lochanski
Metalmax
Search for other works by this author on:
Published:
1993
Page range:
197 - 200

Abstract

Catastrophic pitting corrosion occurred in type 304L stainless steel pipe flange assemblies in an industrial food processor. During regular service the pumped medium was pureed vegetables. In situ maintenance procedures included cleaning of the assemblies with a sodium hypochlorite solution. It was determined that the assemblies failed due to an austenite-martensite galvanic couple activated by a chlorine bearing electrolyte. The martensitic areas resulted from a transformation during cold-forming operations. Solution annealing after forming, revision of the design of the pipe flange assemblies to eliminate the forming operation, and removal of the source of chlorine were recommended.

You do not currently have access to this content.
Don't already have an account? Register

Edward C. Lochanski, 1993. "Galvanic Corrosion Failure of Austenitic Stainless Steel Pipe Flange Assemblies", Handbook of Case Histories in Failure Analysis, Khlefa A. Esaklul

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal