Failure of a Stainless Steel Tank Used for Storage of Heavy Water/Helium

By
R.K. Dayal
R.K. Dayal
J.B. Gnanamoorthy, Indira Gandhi Centre for Atomic Research
Search for other works by this author on:
;
N. Chandrasekharan
N. Chandrasekharan
formerly at Madras Atomic Power Project
Search for other works by this author on:
Published:
1993
Page range:
253 - 255

Abstract

The dished ends of a heavy water/helium storage tank manufactured from 8 mm (0.3 in.) thick type 304 stainless plate leaked during hydrotesting. Repeated attempts at repair welding did not alleviate the problem. Examination of samples from one dished end revealed that the cracking was confined to the heat affected zone (HAZ) surrounding circumferential welds and, to a lesser extent, radial welds that were part of the original construction. Most of the cracks initiated and propagated from the inside surface of the dished ends. Microstructures of the base metal, HAZ, and weld metal indicated severe sensitization in the HAZ due to high heat input during welding. An intergranular corrosion test confirmed the observations. The severe sensitization was coupled with residual stresses and exposure of the assembly to a coastal atmosphere during storage prior to installation. This combination of factors resulted in failure by stress-corrosion cracking. Implementation of a new repair procedure was recommended. Repairs were successfully made using the new procedure, and all cracks in the weld repair zones were eliminated.

You do not currently have access to this content.
Don't already have an account? Register

R.K. Dayal, N. Chandrasekharan, 1993. "Failure of a Stainless Steel Tank Used for Storage of Heavy Water/Helium", Handbook of Case Histories in Failure Analysis, Khlefa A. Esaklul

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal