Skip to Main Content
ASM Failure Analysis Case Histories

Handbook of Case Histories in Failure Analysis

Edited by
Khlefa A. Esaklul
Khlefa A. Esaklul
Search for other works by this author on:
ASM International
Volume
2
ISBN electronic:
978-1-62708-215-0
Publication date:
1993
Book Chapter

Dezincification of a Chrome-Plated Cylinder Gas Valve

By
Richard L. Colwell
Richard L. Colwell
Air Products and Chemicals
Search for other works by this author on:
Published:
1993
Page range:
359 - 361

Abstract

Two new chrome-plated CDA 377 brass valves intended for inert gas service failed on initial installation. After a pickling operation to clean the metal, the outer surfaces of the valves had been flashed with copper and then plated with nickel and chromium for aesthetic purposes. One of the valves failed by dezincification. The porous copper matrix could not sustain the clamping loads imposed by tightening the pressure relief fitting. The second valve failed by shear overload of the pressure relief fitting. Overload was facilitated by a reduction of cross-sectional area caused by intergranular attack and slight dezincification of the inner bore surface of the fitting. Dezincification and intergranular attack were attributed to excessive exposure to nonoxidizing acids in the pickling bath.

You do not currently have access to this content.
Don't already have an account? Register

Richard L. Colwell, 1993. "Dezincification of a Chrome-Plated Cylinder Gas Valve", Handbook of Case Histories in Failure Analysis, Khlefa A. Esaklul

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal