Failed Missile Launcher Detent Spring

By
Gary Wechsler
Gary Wechsler
United States Army Research Laboratory
Search for other works by this author on:
;
Victor K. Champagne
Victor K. Champagne
United States Army Research Laboratory
Search for other works by this author on:
;
Marc Pepi
Marc Pepi
United States Army Research Laboratory
Search for other works by this author on:
Published:
1993
Page range:
455 - 458

Abstract

A missile detached from a Navy fighter jet during a routine landing on an aircraft carrier deck because of a faulty missile launcher detent spring. Visual inspection of Inconel 718 detent spring assembly revealed that four of the nine spring leafs comprising the assembly were plastically deformed while two of the deformed leafs did not meet minimal hardness or tensile requirements. Liquid penetrant testing revealed no cracks or other surface discontinuities on the leaf springs. Material sectioned from the soft spring leafs was heat-treated according to specifications in the laboratory. The resultant increase in mechanical properties of the re-heat-treated material indicated that the original heat treatment was not performed correctly. The failure was attributed to improper heat treatment. Recommendations focused on more stringent quality control of the heat-treat operations.

You do not currently have access to this content.
Don't already have an account? Register

Gary Wechsler, Victor K. Champagne, Marc Pepi, 1993. "Failed Missile Launcher Detent Spring", Handbook of Case Histories in Failure Analysis, Khlefa A. Esaklul

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal