Corrosion Failure of Stainless Steel Components During Surface Pretreatment

By
R.K. Dayal
R.K. Dayal
Reactor Group, Indira Gandhi Centre for Atomic Research
Search for other works by this author on:
;
J.B. Gnanamoorthy
J.B. Gnanamoorthy
Reactor Group, Indira Gandhi Centre for Atomic Research
Search for other works by this author on:
;
Metallurgy Division
Metallurgy Division
Reactor Group, Indira Gandhi Centre for Atomic Research
Search for other works by this author on:
;
G. Srinivasan
G. Srinivasan
Reactor Group, Indira Gandhi Centre for Atomic Research
Search for other works by this author on:
Published:
1993
Page range:
506 - 508

Abstract

Two AISI type 316 stainless steel components intended for use in a reducer section for sodium piping in a fast breeder test reactor were found to be severely corroded—the first soon after pickling, and the second after passivation treatments. Metallographic examination revealed that one of the components was in a highly sensitized condition and that the pickling and passivation had resulted in severe intergranular corrosion. The other component was fabricated from thick plate and, after machining, the outer surface represented the transverse section of the original plate. Pickling and passivation resulted in severe pitting because of end-grain effect. Strict control of heat treatment parameters to prevent sensitization and modification of pickling and passivating conditions for machined components were recommended.

You do not currently have access to this content.
Don't already have an account? Register

R.K. Dayal, J.B. Gnanamoorthy, Metallurgy Division, G. Srinivasan, 1993. "Corrosion Failure of Stainless Steel Components During Surface Pretreatment", Handbook of Case Histories in Failure Analysis, Khlefa A. Esaklul

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal