Failure of a Service Water Pump Shaft

By
Hasan Shaikh
Hasan Shaikh
Metallurgy Division, Indira Gandhi Center for Atomic Research
Search for other works by this author on:
;
H.S. Khatak
H.S. Khatak
Metallurgy Division, Indira Gandhi Center for Atomic Research
Search for other works by this author on:
;
J.B. Gnanamoorthy
J.B. Gnanamoorthy
Metallurgy Division, Indira Gandhi Center for Atomic Research
Search for other works by this author on:
Published:
1993
Page range:
345 - 347

Abstract

A service water pump in a nuclear reactor failed when its shaft gave way. The fracture originated in the threaded portion of the sleeve nut on the drive-end side of the shaft. Results of the failure analysis showed that the cracking initiated at the thread root as a result of corrosion fatigue. Crack propagation occurred either by corrosion or mechanical fatigue. Evidence was found indicating high rotary bending stresses on the shaft during operation. The nonstandard composition of the En 8 steel used in the shaft and irregular maintenance reduced the life of the shaft. Recommendations included use of a case-hardened En 8 steel with the correct composition and regular maintenance of the pump.

You do not currently have access to this content.
Don't already have an account? Register

Hasan Shaikh, H.S. Khatak, J.B. Gnanamoorthy, 1993. "Failure of a Service Water Pump Shaft", Handbook of Case Histories in Failure Analysis, Khlefa A. Esaklul

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal