Skip to Main Content
ASM Failure Analysis Case Histories

Handbook of Case Histories in Failure Analysis

Edited by
Khlefa A. Esaklul
Khlefa A. Esaklul
Search for other works by this author on:
ASM International
Volume
2
ISBN electronic:
978-1-62708-215-0
Publication date:
1993
Book Chapter

Failure Analysis of a Helicopter Main Rotor Bolt

By
Mohan D. Chaudhari
Mohan D. Chaudhari
Columbus Metallurgical Services, Inc.
Search for other works by this author on:
Published:
1993
Page range:
392 - 393

Abstract

A helicopter main rotor bolt failed in the black-coated region between the threads and the taper section of the shank during assembly. The torque applied was approximately 100 N·m (900 in.·lbf) when the bolt sheared. No other bolts were reported to have failed. The failed bolt material conformed to AISI E4340 steel, as specified. The microstructure was tempered martensite, with hardness ranging from 41 to 45 HRC. Failure was in the shear ductile mode. The crack initiated in the area of slag inclusions. Inspection of other bolts from the same shipment was recommended.

You do not currently have access to this content.
Don't already have an account? Register

Mohan D. Chaudhari, 1993. "Failure Analysis of a Helicopter Main Rotor Bolt", Handbook of Case Histories in Failure Analysis, Khlefa A. Esaklul

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal