Failure of an I-Beam

By
R.K. Dayal
R.K. Dayal
Indira Gandhi Centre for Atomic Research
Search for other works by this author on:
;
J.B. Gnanamoorthy
J.B. Gnanamoorthy
Indira Gandhi Centre for Atomic Research
Search for other works by this author on:
;
P. Rodriguez
P. Rodriguez
Indira Gandhi Centre for Atomic Research
Search for other works by this author on:
Published:
1992
Page range:
378 - 381

Abstract

An I-beam of IS-226 specification—I-section dimensions of 450 x l50 x 10 mm (17.7 x 5.9 x 0.4 in.) and a length of 12.41 m (40.7ft)—was flame cut into two section in an open yard near these a coast under normal weather conditions. After approximately 112h, the shorter section of he I-beam split catastrophically along the entire length through the web. Detailed investigation revealed segregation of high levels of carbon, sulfur and phosphorus in the middle of the web and high residual stresses attributed to rolling during fabrication. Flame cutting caused a change in the distribution of the residual stresses, which, aided by low fracture toughness due to the poor quality of the beam, resulted in failure. It was recommended that segregation be avoided in cast ingots used for I-beam manufacture by implementing a better quality-control procedure.

You do not currently have access to this content.
Don't already have an account? Register

R.K. Dayal, J.B. Gnanamoorthy, P. Rodriguez, 1992. "Failure of an I-Beam", Handbook of Case Histories in Failure Analysis, Khlefa A. Esaklul

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal