Intergranular Corrosion Failure in Zn-Al Alloy Solenoid Valve Seats

By
T. Jayakumar
T. Jayakumar
Metallurgy and Materials Progamme, Indira Gandhi Centre for Atomic Research
Search for other works by this author on:
;
D.K. Bhattacharya
D.K. Bhattacharya
Metallurgy and Materials Progamme, Indira Gandhi Centre for Atomic Research
Search for other works by this author on:
;
Baldev Raj
Baldev Raj
Metallurgy and Materials Progamme, Indira Gandhi Centre for Atomic Research
Search for other works by this author on:
;
P. Rodriguez
P. Rodriguez
Metallurgy and Materials Progamme, Indira Gandhi Centre for Atomic Research
Search for other works by this author on:
Published:
1992
Page range:
421 - 423

Abstract

Extensive cracking was found in a batch of die-cast ZAMAK 3 solenoid valve seats during commissioning of the system in which they were installed. Scanning electron microscopic and chemical analyses conducted on one of the failed valve seats showed that the composition of the alloy was different from that specified. The presence of excess aluminum and lead impurities that had segregated to the grain boundaries, coupled with an inadequate amount of magnesium, resulted in intergranular corrosion and subsequent intergranular failure. Corrosion was accelerated by storage in a humid environment in a coastal area. It was recommended that proper chemical analysis of the zinc-aluminum alloy be carried out as a quality control procedure.

You do not currently have access to this content.
Don't already have an account? Register

T. Jayakumar, D.K. Bhattacharya, Baldev Raj, P. Rodriguez, 1992. "Intergranular Corrosion Failure in Zn-Al Alloy Solenoid Valve Seats", Handbook of Case Histories in Failure Analysis, Khlefa A. Esaklul

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal