Book Chapter

Cracking of Aluminum Alloy Aircraft Undercarriage Forgings

By
J.O. Edwards
J.O. Edwards
Metals Technology Laboratories, CANMET
Search for other works by this author on:
;
W.A. Pollard
W.A. Pollard
Metals Technology Laboratories, CANMET
Search for other works by this author on:
;
J.J. Sebisty
J.J. Sebisty
Metals Technology Laboratories, CANMET
Search for other works by this author on:
Published:
1992
Page range:
12 - 16

Abstract

Two complete aircraft undercarriage-leg 2014 aluminum alloy forgings and a number of sectional ends that exhibited cracks during nondestructive testing were examined to determine the extent of damage and the type of cracking. Cracks were primarily confined to the diaphragm and adjoining wall between the steel sleeve and the steel diaphragm washer. Metallographic analysis and accelerated corrosion tests showed that the cracks had originated as stress-corrosion failures.

You do not currently have access to this content.
Don't already have an account? Register

J.O. Edwards, W.A. Pollard, J.J. Sebisty, 1992. "Cracking of Aluminum Alloy Aircraft Undercarriage Forgings", Handbook of Case Histories in Failure Analysis, Khlefa A. Esaklul

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal