Skip to Main Content
ASM Failure Analysis Case Histories

Handbook of Case Histories in Failure Analysis

Edited by
Khlefa A. Esaklul
Khlefa A. Esaklul
Search for other works by this author on:
ASM International
Volume
1
ISBN electronic:
978-1-62708-214-3
Publication date:
1992
Book Chapter

Fatigue Failure of a Carburized Steel Gear From a Helicopter Transmission

By
Martin Roth
Martin Roth
Department of National Defence
Search for other works by this author on:
;
Karen Sander
Karen Sander
Department of National Defence
Search for other works by this author on:
Published:
1992
Page range:
228 - 230

Abstract

The failure of a spiral bevel gear from the transmission of a helicopter was discovered when the transmission was removed after an in-flight incident. Two adjacent teeth from the carburized AISI 9310 steel gear were found to have undergone fatigue failure. Internal initiation occurred in a region depleted of chromium and nickel. This condition coincides with a microstructural inhomogeneity consisting of large, soft ferrite grains. Its origin was probably contamination of the solidifying ingot during the consumable vacuum arc remelting operation.

You do not currently have access to this content.
Don't already have an account? Register

Martin Roth, Karen Sander, 1992. "Fatigue Failure of a Carburized Steel Gear From a Helicopter Transmission", Handbook of Case Histories in Failure Analysis, Khlefa A. Esaklul

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal