Skip to Main Content
ASM Failure Analysis Case Histories

Handbook of Case Histories in Failure Analysis

Edited by
Khlefa A. Esaklul
Khlefa A. Esaklul
Search for other works by this author on:
ASM International
Volume
1
ISBN electronic:
978-1-62708-214-3
Publication date:
1992
Book Chapter

Fatigue Fracture of Stainless Steel Wires in an Electrostatic Precipitator at a Paper Plant

By
Charlie R. Brooks
Charlie R. Brooks
Materials Science and Engineering Department, University of Tennessee
Search for other works by this author on:
Published:
1992
Page range:
218 - 222

Abstract

Several type 316L stainless steel wires in an electrostatic precipitator at a paper plant fractured in an unexpectedly short time. Failed wires were examined using optical and scanning electron microscope, and hardness tests were conducted. Fractography clearly established that fracture was caused by fatigue originating at corrosion pits on the surface of the wire. It was recommended that higher-molybdenum steel in the annealed condition be used to combat pitting corrosion.

You do not currently have access to this content.
Don't already have an account? Register

Charlie R. Brooks, 1992. "Fatigue Fracture of Stainless Steel Wires in an Electrostatic Precipitator at a Paper Plant", Handbook of Case Histories in Failure Analysis, Khlefa A. Esaklul

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal