Skip to Main Content
ASM Failure Analysis Case Histories

Handbook of Case Histories in Failure Analysis

Edited by
Khlefa A. Esaklul
Khlefa A. Esaklul
Search for other works by this author on:
ASM International
Volume
1
ISBN electronic:
978-1-62708-214-3
Publication date:
1992
Book Chapter

Hydrotest Failure of a Carbon Steel Pressure Vessel[1]

By
William R. Warke
William R. Warke
Amoco Corporation
Search for other works by this author on:
Published:
1992
Page range:
143 - 146

Abstract

A carbon steel (ASTM A515 grade 70) pressure vessel failed by brittle fracture while being hydro tested in the fabricating shop. The fracture origin was a small crack at a welding arc strike associated with the toe of a nozzle weld. A fracture mechanics calculation indicated that this imperfection, although small, initiated fracture because of the local geometry and stress conditions and the low toughness of the steel. It was recommended that (1) the probability of flaws be reduced by welding over or grinding out arc strikes, (2) the local stresses be lowered by post weld stress relief and improved weld toe geometry, and (3) toughness be improved by specifying fine-grain steel and/ or by normalizing.

You do not currently have access to this content.
Don't already have an account? Register

William R. Warke, 1992. "Hydrotest Failure of a Carbon Steel Pressure Vessel", Handbook of Case Histories in Failure Analysis, Khlefa A. Esaklul

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal