Anodizing produces a uniform, continuous, highly ordered network of individual cells comprising a layer whose thickness and cell dimensions, and ultimately engineering properties, depend on the electrochemical parameters of the anodizing process. This article discusses the nucleation and growth of anodic aluminum oxide and the important characteristics of the finished porous anodic aluminum oxide. In industry, anodic oxides and the anodizing processes have been categorized into types that exhibit specific properties to suit specific applications. The article reviews the two most basic types of oxides, namely, barrier-layer anodic oxides and porous anodic oxides. It concludes with a description of postanodizing processes, such as dyeing and sealing.

You do not currently have access to this chapter.
Don't already have an account? Register

Jude Mary Runge, 2018. "Anodizing", Aluminum Science and Technology, Kevin Anderson, FASM, John Weritz, J. Gilbert Kaufman, FASM

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal