This article describes the Bayer process for the purification of alumina. The process includes four major stages: digestion, clarification, precipitation, and calcination. The article discusses the aluminum electrolytic process in terms of aluminum electrolysis cell design, magnetohydrodynamic forces, and cathode lining. It reviews the electrochemical reactions and thermodynamics for aluminum electrolysis. The article also describes the cell operations and cell stability, as well as the key indicators of cell performance. It schematically illustrates the typical costs producing aluminum in an aluminum smelter. The article also discusses various environmental issues, such as fluoride recovery; perfluorocarbons, polycyclic aromatic hydrocarbons, and sulfur emissions; spent pot lining; and development of inert anodes and CO2 emissions.

You do not currently have access to this chapter.
Don't already have an account? Register

Alton T. Tabereaux, 2018. "Production of Primary Aluminum by Electrolysis", Aluminum Science and Technology, Kevin Anderson, FASM, John Weritz, J. Gilbert Kaufman, FASM

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal