Skip to Main Content
ASM Handbook

Aluminum Science and Technology

Edited by
Kevin Anderson, FASM
Kevin Anderson, FASM
Mercury Marine
Search for other works by this author on:
;
John Weritz
John Weritz
Aluminum Association
Search for other works by this author on:
;
J. Gilbert Kaufman, FASM
J. Gilbert Kaufman, FASM
Kaufman Associates
Search for other works by this author on:
ASM International
Volume
2A
ISBN electronic:
978-1-62708-207-5
Publication date:
2018
Book Chapter

Lost Foam Casting[1]

By
Kevin Anderson
Kevin Anderson
Mercury Marine
Search for other works by this author on:
Published:
2018
Page range:
232 - 241
Publication history
November 22, 2018

Abstract

Lost foam casting is a sand casting process that uses an expandable polystyrene (EPS) pattern that embodies the positive shape of the part to be cast. Lost foam casting is especially suitable for fairly complex castings with many internal passages. This article discusses the advantages and the process technique of lost foam casting. It describes the pattern molding for the lost foam process that is grouped into four major functions: filling, fusion, cooling (stabilization), and ejection. The article provides information on the application of the pattern coating. It concludes with a review of the quality of the lost foam casting in terms of dimensional tolerances, fold defects, and porosity.

You do not currently have access to this content.
Don't already have an account? Register

Kevin Anderson, 2018. "Lost Foam Casting", Aluminum Science and Technology, Kevin Anderson, FASM, John Weritz, J. Gilbert Kaufman, FASM