In general, metal-matrix composites (MMCs) are classified into three broad categories: continuous fiber-reinforced composites, discontinuous or short fiber-reinforced composites, and particle-reinforced composites. This article focuses on stir casting and melt infiltration as the two main methods of MMC solidification processing. It describes the MCC casting methods, such as sand and permanent mold casting, centrifugal casting, compocasting, and high-pressure die casting. The article discusses the MMC infiltration processes in terms of pressure infiltration casting and liquid metal infiltration. It reviews the powder metallurgy processing of aluminum MMCs and deformation processing of discontinuously reinforced aluminum composites. The article concludes with a discussion on the processing of fiber-reinforced aluminum.

You do not currently have access to this chapter.
Don't already have an account? Register

W.C. Harrigan, Jr., 2018. "Processing of Aluminum Metal-Matrix Composites", Aluminum Science and Technology, Kevin Anderson, FASM, John Weritz, J. Gilbert Kaufman, FASM

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal