Mechanical finishes usually can be applied to aluminum using the same equipment used for other metals. This article describes the two types of grinding used in mechanical finishing: abrasive belt grinding and abrasive wheel grinding. It reviews the binders and fluid carriers used in buffing, and discusses satin finishing and barrel finishing. It also describes lapping and honing techniques that are of special interest in treating aluminum parts that have received hard anodic coatings. Honing recommendations for aluminum alloys are presented in a table.