Abstract

This article presents a summary of aluminum temper designations, and applicable aluminum alloys and product forms for temper designations used in the United States (ANSI H35.1), Europe (EN 515), and internationally (ISO 2107).

You do not currently have access to this chapter.
Don't already have an account? Register

Summary of Aluminum Temper Designations, Aluminum Science and Technology, Vol 2A, ASM Handbook, Edited By Kevin Anderson, FASM, John Weritz, J. Gilbert Kaufman, FASM, ASM International, 2018, p 811–814, https://doi.org/10.31399/asm.hb.v02a.a0006531