Abstract

Brazing technology is continually advancing for a variety of metals including aluminum and its alloys and nonmetals. This article discusses the key physical phenomena in aluminum brazing and the materials for aluminum brazing, including base metals, filler metals, brazing sheet, and brazing flux. It describes various aluminum brazing methods, such as furnace, vacuum, dip, and torch brazing. Friction, flow, induction, resistance, and diffusion brazing are some alternate brazing methods discussed. The article reviews the brazing of aluminum to ferrous alloys, aluminum to copper, and aluminum to other nonferrous metals. It also discusses post-braze processes in terms of post-braze heat treatment and finishing. The article concludes with information on the safety precautions considered in brazing aluminum alloys.