Volume 2A is a practical guide to aluminum and its engineering applications. It begins with a review of temper designations and product forms and the underlying physical metallurgy of aluminum alloys. It then examines manufacturing practices and techniques, focusing in critical areas such as casting, metalworking, heat treating, machining and finishing, surface treatment, and joining. It describes melt and solidification processes, high-integrity die casting, forging, extrusion, powder and additive methods, and the production and use of aluminum foams. The volume also discusses quenching, anodizing, organic and conversion coating, brazing, and laser welding, and offers insights on process selection, quality, performance, service ability, and other product lifetime concerns. For information on the print version of Volume 2A, ISBN: 978-1-62708-207-5, follow this link.
Download citation file:
Close
Table of Contents
-
Introduction
-
Aluminum Alloy Nomenclature and Temper Designations[1]ByJohn WeritzJohn WeritzRevising authorAluminum AssociationSearch for other works by this author on:
-
Properties of Pure Aluminum[1]ByJ. Gilbert KaufmanJ. Gilbert KaufmanKaufman AssociatesSearch for other works by this author on:
-
Physical Metallurgy of Aluminum Alloys[1]ByJunsheng WangJunsheng WangBeijing Institute of TechnologySearch for other works by this author on:
-
-
Aluminum Production and Recycling
-
Production of Primary Aluminum by ElectrolysisByAlton T. TabereauxAlton T. TabereauxAlton Tabereaux ConsultantSearch for other works by this author on:
-
Recycling of AluminumByMark E. SchlesingerMark E. SchlesingerMissouri University of Science and TechnologySearch for other works by this author on:
-
Aluminum Alloy Ingot Casting and Continuous Processes[1]ByJunsheng WangJunsheng WangRevising authorKaiser AluminumSearch for other works by this author on:
-
-
Melting and Shape Casting
-
Die CastingBy
-
Sand Casting of Aluminum AlloysByKumar Sadayappan;Kumar SadayappanCanmet Materials, NrcanSearch for other works by this author on:Abdallah ElsayedAbdallah ElsayedUniversity of GuelphSearch for other works by this author on:
-
Metalworking
-
Work Hardening and Annealing of Aluminum Alloys[1]ByRalph DorwardRalph DorwardRevising authorKaiser AluminumSearch for other works by this author on:
-
Forging of Aluminum Alloys[1]ByTiffany A. DuxTiffany A. DuxArconic Forgings & ExtrusionsSearch for other works by this author on:
-
Forming of Aluminum AlloysByVictoria BurtVictoria BurtRevising authorASM InternationalSearch for other works by this author on:
-
Process Technologies for Powder, Composite, Foam, and Semisolid Product Forms
-
Processing of Aluminum Metal-Matrix Composites[1]ByW.C. Harrigan, Jr.W.C. Harrigan, Jr.Revising authorMMC Engineering, Inc.Search for other works by this author on:
-
Aluminum Foams—Processing, Properties, and ApplicationsByJ. Baumeister;J. BaumeisterFraunhofer Institute for Manufacturing Technology and Advanced MaterialsSearch for other works by this author on:D. Lehmhus;D. LehmhusFraunhofer Institute for Manufacturing Technology and Advanced Materials and MAPEX Center for Materials and Processes at University of BremenSearch for other works by this author on:J. WeiseJ. WeiseFraunhofer Institute for Manufacturing Technology and Advanced MaterialsSearch for other works by this author on:
-
Semisolid Metal CastingByStephen P. MidsonStephen P. MidsonThe Midson Group, Inc. and Colorado School of MinesSearch for other works by this author on:
-
Heat Treatment
-
Metallurgy of Heat Treatable Aluminum AlloysByD. Scott MacKenzieD. Scott MacKenzieHoughton InternationalSearch for other works by this author on:
-
Quenching of Aluminum Alloys[1]ByD. Scott MacKenzieD. Scott MacKenzieHoyghton InternationalSearch for other works by this author on:
-
Heat Treatment Practice of Wrought Age-Hardenable Aluminum AlloysByD.S. MacKenzieD.S. MacKenzieHoughton InternationalSearch for other works by this author on:
-
-
Machining and Mechanical Finishing
-
Machining of Aluminum AlloysByMichael E. FinnMichael E. FinnFinn Metalworking and Cutting SolutionsSearch for other works by this author on:
-
Laser Beam Machining of Aluminum and Aluminum AlloysByMangesh V. Pantawane;Mangesh V. PantawaneUniversity of North TexasSearch for other works by this author on:Sameehan S. Joshi;Sameehan S. JoshiUniversity of North TexasSearch for other works by this author on:Narendra B. DahotreNarendra B. DahotreUniversity of North TexasSearch for other works by this author on:
-
Mechanical Finishing of Aluminum[1]ByMichael E. FinnMichael E. FinnFinn Metalworking and Cutting SolutionsSearch for other works by this author on:
-
-
Cleaning and Surface Treatment
-
Metallurgy Basics for Aluminum Surface TreatmentByJude Mary Runge;Jude Mary RungeCompCote International, Inc.Search for other works by this author on:
-
Chemical and Electrolytic Brightening[1]ByWayne ChandlerWayne ChandlerSIC Technologies, Inc.Search for other works by this author on:
-
Etching of Aluminum and Its AlloysByLinda NewmanLinda NewmanHoughton InternationalSearch for other works by this author on:
-
AnodizingByJude Mary RungeJude Mary RungeCompCote International, Inc.Search for other works by this author on:
-
Plating on Aluminum[1]ByJude Mary Runge;Jude Mary RungeCompCote International, Inc.Search for other works by this author on:
-
Porcelain Enameling of Aluminum AlloysByCullen L. HacklerCullen L. HacklerPorcelain Enamel Institute, Inc.Search for other works by this author on:
-
-
Joining
-
Weldability of Aluminum Alloys[1]ByPatrick BerubePatrick BerubeHobart Brothers Co.Search for other works by this author on:
-
Arc Welding of Aluminum Alloys[1]ByDevan DePauwDevan DePauwNorthwestern Michigan CollegeSearch for other works by this author on:
-
Laser Welding of Aluminum AlloysByShuang LiuShuang LiuMiller Electric Mfg. Co.Search for other works by this author on:
-
Laser Stir WeldingByRichard Martukanitz;Richard MartukanitzPennsylvania State UniversitySearch for other works by this author on:Israel StolIsrael StolConsultant and retired from Alcoa Technical CenterSearch for other works by this author on:
-
Friction Stir Welding of Aluminum AlloysByKevin ColliganKevin ColliganAIT Nova-Tech Engineering, LPSearch for other works by this author on:
-
Brazing of Aluminum AlloysByD.P. SekulicD.P. SekulicUniversity of Kentucky and Harbin Institute of TechnologySearch for other works by this author on:
-
Adhesive Bonding[1]ByVictoria BurtVictoria BurtRevising authorASM InternationalSearch for other works by this author on:
-
Mechanical Joining of AluminumByToby PadfieldToby PadfieldAmerican Axle & Manufacturing, Advanced Technology Development CenterSearch for other works by this author on:
-
-