This article is an atlas of fractographs that helps in understanding the causes and mechanisms of fracture of metal-matrix composites, including tungsten fiber-reinforced aluminum, tungsten fiber-reinforced carbon steel, and tungsten fiber-reinforced silver. The fractographs illustrate the ductile fracture, interlaminar failure, transgranular cleavage and fracture, tension-overload fracture, longitudinal and transverse cracking, fiber splitting, stress rupture, and low-cycle fatigue of these composites.