This article is an atlas of fractographs that helps in understanding the causes and mechanisms of fracture of cobalt alloys (cast Vitallium and cast ASTM F75 alloys) and in identifying and interpreting the morphology of fracture surfaces. The fractographs illustrate the fatigue fracture, microcrack, and stair-step fracture surface of these alloys.